Acrylic Polishing & Surface Finishing | Beaulic

Clarity you can measure

For optical and diagnostic parts, “looks clear” is not a specification. We finish to measurable targets — roughness, flatness and transmission — and report the numbers with the shipment.

Capability 04 — Polishing & Surface Finishing

From machining marks to optical surfaces

Polishing is a controlled material-removal process, not cosmetic buffing. Over-polish changes geometry; under-polish leaves scatter sources. We qualify the route per part family and measure the result.

  • Flame & vapor polishing to restore transparency after machining without rounding critical edges.
  • Optical lapping for flatness below 2 µm over 50 mm and Ra ≤ 0.02 µm.
  • Annealing to relieve machining stress and eliminate later solvent-crack failures.
  • Functional coatings light-blocking, anti-scratch and anti-reflection options applied where the application needs them.
Discuss your part
Polishing an acrylic optical surface
Process route

How we run it, step by step

Specifications

Process envelope

Typical values. Tighter limits are available after a drawing review — share the functional requirement rather than a blanket tolerance.

Parameter Standard Precision / achievable Notes
Surface roughnessRa 0.4 µmRa 0.02 µmOptical lapping or diamond fly-cutting
Flatness after finishing20 µm / 100 mm2 µm / 50 mmOn lapped optical faces
Transmission (PMMA, 3 mm)92% typicalon requestMeasured per agreed wavelength range
Edge clarity (laser or polished)visual acceptancephotometricDefined per drawing on request
Coating optionslight-blocking, anti-scratchAR on requestAdhesion tested per lot
Annealingstandard for bonded parts—Cycle recorded in lot file
Applications

Where this process earns its keep

  • Lenses & light guides Machined and polished PMMA optics with documented transmission.
  • Diagnostic windows & cuvettes Low-scatter surfaces for absorbance and fluorescence measurements.
  • Display covers & panels Anti-scratch, anti-glare finishes with controlled haze.
  • Fluidic channel interiors Vapor-polished channels that reduce particulate adhesion.
Polished acrylic lenses and light guides

Send the drawing, get a process answer